Comprehensive Optical Inspection for PET Preforms

Delta Engineering teams with Intravis to inspect preform mouth, body, thread and color.

Share

During the recent K 2022 show in Düsseldorf, Delta Engineering of Belgium (U.S. office in Norcross, Ga.) showed of its new DCI 500 optical inspection system for PET preforms. It incorporates various inspection stations from the Intravis PreWatcher Offline system. The DCI 500 inspects the preform mouth, inspects the body and thread for contamination, and performs color inspection using a spectrometer. This system was demonstrated at the Düsseldorf plant of Nissei ASB Machine Co. during the show.

At K 2022, Delta Engineering also introduced a multifunctional inline test system for blow molded containers.

Related Content

Advantage temperature control units
Konica Minolta
FormNext Chicago
See FasTie at NPE2024 in Smartflow Booth W3071
HAIDLMAIR NPE2024
large tonnage injection molding productivity
Shell Polymers (Real)ationships start here ad
structural foam molding chemical foaming agents
Shell Polymers (Real)ationships start here ad.