Share

Recent research conducted by Farrel Pomini, FPInnovations and a consortium of industry leaders have reportedly demonstrated the commercial viability of biobased, compostable compounds such as polylactic acid (PLA) and polyhydroxyalkanoates (PHA) mixed with high levels of fiber in a variety of disposable packaging products, paving the way for eco-friendly products like food trays and disposable cutlery (Figure 1).

Compounding equipment builder Farrel Pomini and Montreal-based FPInnovations, the world’s largest nonprofit research technology organization for forestry, have proven the technology to produce industrial-grade biobased compounds with fiber content up to 60%. The compounds, produced on the Farrel Continuous Mixer, have been used to manufacture various products, including injection-molded disposable knives with up to 40% fiber, extruded sheets and thermoformed parts with fiber content ranging from 0.5% to 10%.

Wood Pulp Compounded in PLA

FIG 1 Applications for bioresin and wood pulp compounds include disposable cutlery. Source: FPInnovations

The final products are odor-free with light coloration, attributed low processing temperatures. Dr. Peng Ye, applications development manager for Farrel Pomini, presented the results of this project in May in Orlando, Florida, during NPE2024.

Leveraging Cellulose From Wood Pulp

Development of these cellulose-filled biodegradable resins is a result of a collaborative effort led by FPInnovations, based in Montreal. Farrel Pomini played a crucial role in producing these compounds at pilot and industrial scales using its continuous mixing technology at its lab in Ansonia, Connecticut.

The key to these innovations lies in using refined wood pulp, sourced for this collaboration from sawmill residue provided by West Fraser, a major wood products company. This refined wood pulp undergoes a process that removes most of the lignin, leaving cellulose and hemicellulose.

The low-lignin content of this wood pulp makes it suitable for food contact applications, and enhances processing conditions and heat resistance. Moreover, its wide commercial availability and inherent compostability make it an well suited for sustainable everyday products solutions, notes Dr. Yann Gabet, FPInnovations’ senior scientist and the project leader for the Biocomposites Initiative.

Farrel Pomini and FP Innovations found that adding cellulose fibers in PLA and PHA compounds provided several advantages, notably:

  • High dispersion quality: The compounds demonstrate excellent dispersion up to 60% cellulose content.
  • Enhanced heat resistance: The heat deflection temperature (HDT) of crystalline PLA-based parts significantly improves with the addition of cellulose fiber, surpassing 100°C with 5% wood pulp and reaching 150°C with 20% pulp content. This makes the compounds suitable for hot food and liquid contact applications (see Figure 2).
  • Mechanical properties: Adding up to 5% wood pulp maintains or enhances tensile modulus, tensile strength and impact resistance without significantly affecting elongation properties (see Figure 3).

Ye and Gabet note that a critical feature of these cellulose-filled PLA compounds is their accelerated biodegradation compared to pure PLA. Testing conducted in accordance with ISO 14855-1 standards showed that PLA compounds with 20% cellulose demonstrated a faster biodegradation rate within the first 25 days compared to PLA alone. Additionally, compounds with 5% of another type of cellulose product achieved 90% biodegradation nearly 30 days earlier than pure PLA.

FIG 2 The heat deflection temperature of crystalline PLA-based parts significantly improves with the addition of cellulose fiber, surpassing 100°C with 5% wood pulp and reaching 150°C with 20% pulp content.
  

Moreover, according to Ye, Farrel Pomini’s compounding technology helps reduce the impact of the compounding process on sensitive materials (like cellulose and biopolymers) by utilizing low processing temperatures. This process also enables a reduction in moisture content from an initial 3% to 4% in the fiber to a final compound moisture of 0.05% to 0.1%.

 
FIG 3 Adding up to 5% wood pulp maintains or enhances tensile modulus, tensile strength and impact resistance without significantly affecting elongation properties.

The Farrel Continuous Mixer (FCM) is a continuous compounder well suited to processing highly filled, temperature/shear-sensitive applications and excels at processing biodegradable plastics in addition to white and black masterbatches, PVC, flooring, halogen-free flame-retardant compounds, and wire and cable applications.

The FCM melts feedstock resins and homogenizes them under specific temperature and pressure parameters. Ye explains that the mixer’s low process temperature, short residence time and efficient rotor shear make it well suited for processing temperature-sensitive materials or materials with prior heat history. The mixer has been used to process PLA, PHA, PBS, recycled PVC and film scrap.

Environmental and Economic Benefits

Incorporating cellulose fibers into biodegradable resins offers several economic and environmental advantages, the partners in this project determine. These include:

  • Lower costs compared to pure biopolymer
  • Improved compostability of final products
  • Optimized mechanical properties
  • Improved heat resistance
  • Lower carbon footprint

States Gabet, “The successful development and scaling of cellulose-filled biodegradable resins highlights a significant leap towards sustainable solutions for plastic-based everyday products. By combining innovative technology with the abundant resource of wood pulp, these advancements offer a practical and environmentally friendly alternative for various applications.”

IMTS+
Become a NTMA member today!
MMS Online Apr-2021
NTMA
NTMA
TD-Series Desiccant Dryers
Glycon's DM2: The High Performance Feedscrew
We ❤ Powders

Related Content

Packaging

How to Extrusion Blow Mold PHA/PLA Blends

You need to pay attention to the inherent characteristics of biopolymers PHA/PLA materials when setting process parameters to realize better and more consistent outcomes.    

Read More
Medical

Medical Molder, Moldmaker Embraces Continuous Improvement

True to the adjective in its name, Dynamic Group has been characterized by constant change, activity and progress over its nearly five decades as a medical molder and moldmaker.

Read More

‘Monomaterial’ Trend in Packaging and Beyond Will Only Thrive

In terms of sustainability measures, monomaterial structures are already making good headway and will evolve even further.

Read More
Packaging

Multilayer Solutions to Challenges in Blow Molding with PCR

For extrusion blow molders, challenges of price and availability of postconsumer recycled resins can be addressed with a variety of multilayer technologies, which also offer solutions to issues with color, processability, mechanical properties and chemical migration in PCR materials.

Read More

Read Next

NPE

Beyond Prototypes: 8 Ways the Plastics Industry Is Using 3D Printing

Plastics processors are finding applications for 3D printing around the plant and across the supply chain. Here are 8 examples to look for at NPE2024.

Read More
NPE

For PLASTICS' CEO Seaholm, NPE to Shine Light on Sustainability Successes

With advocacy, communication and sustainability as three main pillars, Seaholm leads a trade association to NPE that ‘is more active today than we have ever been.’    

Read More
MMS ad