PlastiComp Expands LFT Pellet Capacity

Increasing customer demand for Complet long-fiber thermoplastic (LFT) pellets has prompted PlastiComp LLC, Winona, Minn., to plan installation of a new production line capable of 3 million to 5 million lb/yr.

Share

Increasing customer demand for Complet long-fiber thermoplastic (LFT) pellets has prompted PlastiComp LLC, Winona, Minn., to plan installation of a new production line capable of 3 million to 5 million lb/yr. The firm is also preparing a new plant site in the Winona area for occupancy next year. Tel: (507) 454-4334 • www.plasticomp.com