AERT (Advanced Environmental Recycling Technologies) Inc. in Springdale, Ark., maker of ChoiceDek wood/plastic composite deck boards, has always had a “green” strategy.

Share

AERT (Advanced Environmental Recycling Technologies) Inc. in Springdale, Ark., maker of ChoiceDek wood/plastic composite deck boards, has always had a “green” strategy. Since it was founded in 1988, its goal has been to turn recycled wood and polyethylene into the highest quality deck boards available anywhere. The company struggled for the first 12 years to get its unusual cold-flow extrusion process to make money. Now with recent moves toward greater efficiency, automation, and economy of scale, AERT is becoming a low-cost producer.

Founder Joe Brooks developed the patented process to ensure 100% encapsulation of wood fiber with plastic before extrusion, which prevents delamination and other problems later. AERT blends recycled wood fiber (much of it from the local furniture industry) with recycled LDPE, LLDPE, and HDPE from film and gable-top milk and juice cartons. After about 1 hr of intensive mixing at 430 F in sequenced batch mixers, the hot plasticated material is sized into 2- to 4-in. chunks and discharged onto a belt to cool before being fed into chilled extruders with heated dies and embossers.

AERT buys only used single-screw extruders and then rebuilds them to its specifications with circulating chilled water and no heater bands. “When boards are cold formed, they have more strength,” says senior v.p. Alford Drinkwater.

Mixing and extrusion is now fully automatic, computerized and monitored from a control room on a different floor from manufacturing. There are no operators at the machines. But as production has grown over the past five years, AERT has doubled its work force to over 600 people.

 

Green and out of the red

AERT has been profitable since 2001 and steadily expanding. A new decking extrusion plant is ramping up production now, which will double AERT’s capacity. The new plant will have four more cold extrusion lines for a total of eight. The first new line is already running.

To reduce floor space for cooling the profiles, AERT devised an accumulator, which occupies a fraction of the floor space taken up by the network of horizontal conveyors in the original plant.

Last year, AERT launched MoistureShield, a new premium decking with deep colors and deep embossing, marketed directly to outlets serving professional contractors. MoistureShield is intended to diversify AERT’s product offerings and reduce its dependence on ChoiceDek, made for Weyerhaeser and distributed through Lowe’s, which is about 90% of AERT’s sales. AERT chairman Brooks says it also plans to introduce an “all-natural, chemical-free” cedar composite deck board next year.

Last year AERT used 125 million lb of recycled PE and the same amount of recycled wood fiber. AERT is adding a third plastic recycling plant and a new process to recycle lower grade film in the form of bags sourced from municipal recycling facilities. AERT plans to invest $45 million over the next five years in a new chopping, washing, and extrusion plant in Oklahoma with initial capacity to reclaim about 75 million lb/yr of bag film. AERT has also developed and filed for patents on new processes to optimize the melt index and density of the recycled bag material.

AERT already has two proprietary recycling processes, one for relatively clean post-consumer and post-industrial LLDPE film, the other to extract LDPE from wet paper pulp left after fiber is recovered from gable-top cartons. Clean film recycling involves grinding, dry separation of contaminants and metal, and then densifying before extrusion. AERT found it needed more rugged and powerful densifiers than those on the market, so the company designed its own and had them custom-built locally. Automatic controls sound a warning if temperature, amperage, or vibration exceeds preset limits.

AERT also built a new wood-fiber processing plant next to the new cold extrusion facility. AERT tests incoming wood fiber for moisture and particle size, grinds it, classifies it by size, then dries and classifies it again. The large rotary dryer is fired by waste wood from the process instead of the natural gas used in AERT’s original fiber plant—a further cost-saving and “green” improvement. 

NTMA
IMTS+
NTMA
MMS Online Apr-2021
Become a NTMA member today!
Resinworks with Optimizer
New CM-17d
Best of the Best

Related Content

Postconsumer

Evolving Opportunities for Ambitious Plastics Recycler

St. Joseph Plastics grew from a simple grinding operation and now pursues growing markets in recycled PP, food-grade recycled materials, and customized post-industrial and post-consumer compounds.

Read More
Postindustrial

Extrusion Technology Extended to Injection, Enabling Up to 100% Regrind Usage

Twin-barrel (shot-pot) press can handle more regrind, offers other benefits to molders.

Read More
Packaging

Multilayer Solutions to Challenges in Blow Molding with PCR

For extrusion blow molders, challenges of price and availability of postconsumer recycled resins can be addressed with a variety of multilayer technologies, which also offer solutions to issues with color, processability, mechanical properties and chemical migration in PCR materials.

Read More
sustainability

Scaling Up Sustainable Solutions for Fiber Reinforced Composite Materials

Oak Ridge National Laboratory's Sustainable Manufacturing Technologies Group helps industrial partners tackle the sustainability challenges presented by fiber-reinforced composite materials.

Read More

Read Next

NPE

Making the Circular Economy a Reality

Driven by brand owner demands and new worldwide legislation, the entire supply chain is working toward the shift to circularity, with some evidence the circular economy has already begun.

Read More
sustainability

Lead the Conversation, Change the Conversation

Coverage of single-use plastics can be both misleading and demoralizing. Here are 10 tips for changing the perception of the plastics industry at your company and in your community.

Read More
NPE

For PLASTICS' CEO Seaholm, NPE to Shine Light on Sustainability Successes

With advocacy, communication and sustainability as three main pillars, Seaholm leads a trade association to NPE that ‘is more active today than we have ever been.’    

Read More
MMS ad