Researchers at U.K.’s University of Birmingham have developed a type of nylon bioplastic that is tough and strong and easy to process for medical implants.
Data from independent labs find Ascend’s Acteev antimirobial technology for surgical masks deactrivates bacteria, fungi and viruses, including SARS-CoV-2.
On the same day of its acquisition of Clariant’s color masterbatches business, PolyOne also announced that going forward, it will be known by the name ‘Avient’.