Fungi Makes Meal of Polypropylene

University of Sydney researchers identify two strains of fungi that can biodegrade hard to recycle plastics like PP.

Share

U. of Sydney researchers identify two fungi strains that successfuly biodegrade polypropylene
Photo Credit: University of Sydney

Ongoing research into a variety of technologies for biodegradation of hard to recycle plastics is among the various avenues being taken by the industry and academia in their efforts to address plastic waste and the circular economy. Recently, two common strains of fungi were used to successfully biodegrade polypropylene in a laboratory experiment led by researchers at Australia’s University of Sydney, School of Chemical & Biomolecular Engineering. On the scary side, some science fiction film lovers might recall Michel Chrichton’s 1968 The Andromeda Strain and the 1971 film of the same name which fictitiously describe a microbe Phantom F-4.  This biological agent recovered from a satellite and subsequently mutated degrades and destroys rubber-like materials in the aircraft including the pilot's oxygen mask, and eventually the pilot as well.

The U. of Sydney researchers focused on polypropylene due to its high volume focused on PP due to its high volume use in such a broad variety of applications ranging from packaging, toys and other consumer goods to furnishings and automotive. They noted that PP   ‘has long been recycling’s head scratching riddle’, and also that PP reportedly accounts for roughly 28% of the world's plastic waste, but only 1% of it is recycled currently. They attributed PP’s infrequent recycling to its short life as a packaging material and because it often becomes contaminated by other materials and plastics, necessitating new recycling methods that have minimal environmental impact.

Overseeing the study, professor Ali Abbas from the School of Chemical & Molecular Engineering and chief circular engineer at Circular Australia said, “Despite the massive scale of plastic production and consumption, there has been very little attention paid to plastics degradation under environmental conditions, and our understanding of how plastics can be degraded is limited. One big question our result has raised is – what are the naturally occurring conditions which can fast track the degradation of plastics? We seek to further explore the role of biological processes offered by fungi and other microorganisms.”

Typically found in soil and plants, the study found that two strains of fungi Aspergillus terreus and Engyodontium album were able to break down PP after it had been pre-treated with either UV light or heat, reducing the plastic by 21% over 30 days of incubation, and by 25%-27% over 90 days.

The researchers hope their method could one day reduce the vast amount of plastic polluting the environment and lead to a greater understanding of how plastic pollution might biodegrade naturally under certain conditions. Said PhD student Amira Farzana Samat and the study’s lead author, “Polypropylene is a common plastic used to make a huge variety of everyday products like food containers, coat hangers and cling film, but it only has a recycling rate of only one percent, meaning it is overrepresented in plastic waste and pollution globally.”

According to co-author of the study professor Dee Carter, an expert in mycology – the study of fungi – in the university’s School of Life & Environmental Sciences, fungi are exceptionally versatile and are known to be able to break down pretty much all substrates. Carter attributes this ‘superpower’ to fungi’s production of powerful enzymes, which are excreted and used to break down substrates into simpler molecules that the fungal cells can then absorb.

Said Carter, “Often, these fungi have evolved to break down woody materials, but this ability can be repurposed to attack other substrates - this is why we find fungi growing on all sorts of man-made materials like carpets, painted furniture, grout around tiles, shower curtains, upholstery and even car headlights. Recent studies suggest some fungi may even degrade some of the ‘forever chemicals’ like PFAS, but the process is slow and not yet well understood. There is also evidence that the amount of plastic accumulated in the ocean is less than what might be expected based on production and disposal levels, and there is speculation that some of this ‘missing’ plastic may have been degraded by marine fungi.”

U. of Sydney researchers identify two fungi strains that biodegrade PP
Photo Credit: University of Sydney

The Method and What’s Next

Polypropylene in various forms was initially treated with one of three separate methods: UV light, heat, and Fenton’s reagent – an acidic solution of hydrogen peroxide and ferrous iron often used to oxidize contaminants.

In a petri dish, the fungi were applied separately as single cultures to treated PP. The validity of the biodeterioration was then confirmed through microscopy techniques. While the research didn’t evaluate how the plastic was degraded by the fungi or whether it was metabolized, the researchers hope to conduct further research to determine the type of biochemical processes taking place.

Professor Abbas, who believes the low rate of plastics recycling globally presents a 'massive plastics circularity gap’ noted, “We need to support the development of disruptive recycling technologies that improve the circularity of plastics, especially those technologies that are driven by biological processes like in our study. It is important to note that our study did not yet carry out any optimization of the experimental conditions, so there is plenty of room to further reduce this degradation time.”

Purgex: Made in the USA. Trusted Globally.
Stop Wasting. Start Shredding
Best of the Best
New 2024 Twin Screw Report
TD-Series Desiccant Dryers
New CM-17d
Register Now!
Glycon's DM2: The High Performance Feedscrew
Elevate your PET sorting
Gardner Business Media, Inc.
Resinworks with Optimizer
Guill - World Leader in Extrusion Tooling

Related Content

resin pricing

Prices of All Five Commodity Plastics On the Way Up

Despite earlier anticipated rollover in prices for most of the volume commodity resins, prices were generally on the way up for all going into the third month of first quarter.  

Read More
Biopolymers

Advanced Biobased Materials Company PlantSwitch Gets Support for Commercialization

With participation from venture investment firm NexPoint Capital, PlantSwitch closes it $8M bridge financing round.

Read More
PET

First Quarter Looks Mostly Flat for Resin Prices

Temporary upward blips don't indicate any sustained movement in the near term.

Read More
Commodity Resins

Prices for All Volume Resins Head Down at End of 2023

Flat-to-downward trajectory for at least this month.

Read More

Read Next

NPE

For PLASTICS' CEO Seaholm, NPE to Shine Light on Sustainability Successes

With advocacy, communication and sustainability as three main pillars, Seaholm leads a trade association to NPE that ‘is more active today than we have ever been.’    

Read More
sustainability

Lead the Conversation, Change the Conversation

Coverage of single-use plastics can be both misleading and demoralizing. Here are 10 tips for changing the perception of the plastics industry at your company and in your community.

Read More
sustainability

See Recyclers Close the Loop on Trade Show Production Scrap at NPE2024

A collaboration between show organizer PLASTICS, recycler CPR and size reduction experts WEIMA and Conair recovered and recycled all production scrap at NPE2024.

Read More
New 2024 Twin Screw Report