Screw Speed vs Recovery Time
Many times the screw speed is not setup to operate at its most effective operation.
Many times I have visited processing facilities to help molders solve one problem or another. In reviewing their setup parameters, I find many times that the screw speed is not setup to operate at its most effective operation.
There have been times, for example, when a customer was processing Xenoy— Sabic’s blend of semi-crystalline polyester (typically polybutylene terephthalate, or PET, and polycarbonate—and the molder was complaining that the screw was degrading the resin. The screw was turning at a fairly moderate speed and was recovering in 5 sec, then sitting in the back position before injecting for an additional 8 sec. Then during the injection stroke, degassing and smoke was evident at the nozzle.
After witnessing several cycles of operation in the above manner, I suggested that the screw rotation be reduced to the point where the screw got back just in time so that a count of “3” could be obtained. Then the screw was stroked forward to fill the mold. The screw speed was practically reduced by half, and within about three shots the degraded material was flushed out of the barrel, and the smoking stopped.
This simple change in the processing parameter reduced the shear on the resin and allowed the process to be improved. Not only was the degrading eliminated, but most of all the overall melt temperature was reduced which in turn reduced the cooling time and, therefore, reduced the overall cycle time.
_______________________________________________________________________________________
Related Content
-
Breaking News From NPE2024
Here is a firsthand report of news in injection molding, extrusion, blow molding and recycling not previously covered.
-
A Recycling Plant, Renewed
Reinvention is essential at Capital Polymers, a toll recycler that has completely transformed its operation in a short period of time.
-
Processing Megatrends Drive New Product Developments at NPE2024
It’s all about sustainability and the circular economy, and it will be on display in Orlando across all the major processes. But there will be plenty to see in automation, AI and machine learning as well.