UV Additive Masterbatch for Clear PET Food Packaging
Ampacet’s PET UVA also preserves the integrity of contents in clear PET and rPET packaging for personal care and household products.
Photo Credit: Ampacet Corp.
A new UV additive masterbatch developed for blow molding, and film and sheet extrusion of clear PET food packaging has been introduced by Ampacet. FDA-approved for food contact, Ampacet’s PET UVA masterbatch is said to protect packaging contents from damaging UV light, keeping food fresher, prolonging product shelf life and reducing waste. It also preserves the integrity of contents in clear PET and rPET packaging for personal care and household products.
PET UVA boasts excellent clarity and UVA protection, with transmission of less than 10% at 13 mils up to 390 nm with a 1% LDR (let-down-ratio). According to Ampacet, this UV masterbatch significantly reduces the cost of UVA protection for PET packaging by providing benefits with LDRs of as low as .4% to .8%, depending on performance requirements.
Related Content
-
Prices Up for PE, ABS, PC, Nylons 6 and 66; Down for PP, PET and Flat for PS and PVC
Second quarter started with price hikes in PE and the four volume engineering resins, but relatively stable pricing was largely expected by the quarter’s end.
-
Part 3: The World of Molding Thermosets
Thermosets were the prevalent material in the early history of plastics, but were soon overtaken by thermoplastics in injection molding applications.
-
Advanced Biobased Materials Company PlantSwitch Gets Support for Commercialization
With participation from venture investment firm NexPoint Capital, PlantSwitch closes it $8M bridge financing round.