Recycling
New Pulverizer Helps PVC Processor Boost Output
New unit from Pallmann converts PVC scrap and delivers 2000 lb/hr of recycled PVC at 20 mesh (840 micron) particle size.
Read MoreA New ‘Supercritical Water’ Approach to Recycling Plastic Packaging Waste
University of Birmingham license the rights to its technology to U.K.’s Stopford to develop a novel process for recycling mixed plastic packaging to obtain high-value recycled plastic.
Read MoreInjection Molder Sees Huge Growth in Recycling
Wittmann Battenfeld's material-handling systems and engineering support helped Monoflo International reprocess more than 60 million lb of plastics over 10 years.
Read MoreVecoplan Opens West Coast Office
Southern California location to provide sales and after-sales support offices, spare and replacement parts, and offer product trials for shredders.
Read MoreHoneywell, Avangard to Build New Advanced Recycling Plant in Texas
The planned advanced recycling plant is expected to have the capacity to transform 30,000 metric tons of mixed waste plastics into Honeywell recycled polymer feedstock per year.
Read MoreSolvent-Based Recycling: Emerging Technology for Reclaiming & Purifying Polyolefins with Twin-Screw Extruders
Just now being applied commercially, solvent-based recycling turns colored polyolefin waste into clear, clean and even food-grade resin comparable to virgin—all while keeping the polymer structure intact. Specially engineered systems of tandem twin-screw or twin- and single-screw extruders can do the trick.
Read MoreDow Invests in Recycler Mr. Green Africa
At full scale, the investment is expected to create approximately 200 more direct jobs, impact the lives of 5,000 waste pickers and engage more than 250,000 consumers in separation at source programs.
Read MoreScrap-Reclaim System For Film
Can reprocess 90-110 lb/hr of PE scrap and is fed via a trim basket and/or optional roll feed.
Read MoreCyclyx to Build Advanced Recycling Plant on Gulf Coast
The facility is expected to process up to 60,000 metric tons of recycled plastic feedstock per year with an anticipated start-up in late 2022.
Read More