Long-Glass PP Makes InroadsIn Automotive Front Ends
Injection molded, long-glass-reinforced polypropylene appears to be the staple of new automotive front-end systems (FES) designed with a high degree of parts integration.
Read MoreNew Methods Expand Roles of Gas-Assist Molding
Two variations on gas-assist injection molding were presented in papers at the Molding 2002 Conference held in New Orleans in March.
Read MoreTwo New Ideas for Injection Molding Unveiled at ANTEC Meeting
A new method of coinjection molding dissimilar materials was presented at this year's SPE Annual Technical Conference in San Francisco.
Read MoreInjection Molding Technologies Advance At Structural Plastics Show
A simpler approach to in-mold film decorating was one new injection molding capability presented at the SPI Structural Plastics show and conference.
Read MoreThe New Polypropylenes - They've Got More of Everything
Whether it’s toughness, stiffness, heat resistance, clarity, barrier properties, high flow, or high melt strength—you’ll find more of what you’re looking for in new breeds of PP resins from all suppliers.
Read MoreWater Injection Molding Makes Hollow Parts Faster, Lighter
Water-assisted injection molding is the newest way to mold hollow or partly hollow parts.
Read MoreLow-Cost Process Makes Crosslinked PE Foam
A new way to make closed-cell, crosslinked polyolefin foam buns uses far less expensive equipment and less energy than conventional processes.
Read More"Electrically Active" Compounds Surge In Performance
Designing a thermoplastic compound to conduct an electrical charge is difficult and costly, since most polymers are naturally ill suited to the task.
Read MoreNew Machinery &Materials Help Rotomolders Add Value to Parts
Producing solid features in an otherwise hollow rotomolded part and coloring parts in easier and more flexible ways are two new developments highlighted at the January meeting of the Association of Rotational Molders (ARM) in Minneapolis.
Read MoreBig German Plant May Relieve U.S. Bottleneck in Recycling Carpet Nylon
An unexpected bottleneck in U.S. nylon recycling could be alleviated by a giant new carpet recycling plant in Germany.
Read More